Technical Description
The present invention relates to a low temperature method for fabrication of dense boron carbide composites. The process consists of sintering of B4C composite at SPS temperature of 1400°C and 50 MPa pressure through spark plasma sintering route using mechanically activated Ti-B reactive mixture as a sintering aid.
Problems Addressed
- Expensive
- High Temperature Sintering
- High Porosity
- Inefficient Fabrication
- Lack of Mechanical Properties
- Limitations of Existing Methods
Tech Features
- Low Temperature Sintering
- Improved Mechanical Properties
- Ease of Fabrication
- B4C composite Synthesis
- Fully Dense Composite
- Low Porosity
Target Audience
- Aerospace and Defense Sector
- Nuclear Power Sector
- Automotive Sector
- Electronics Industry
- Research & Development
Tech ID: P03-1719 TRL 3 Patent Status: Granted Available For Exclusive and Non-exclusive License
×